 RTV-2 Silicone for molding applications:
RTV-2 Silicone rubber for plaster statue molding making is primarily intended forstatues Buddha, artifacts copied, building decoration materials, large-scale cement mold, artificial fossils Factory,Europe component factory, simulation landscapes, animals and plants sculpture, sandstone crafts ,poly resin crafts,PU crafts,PU resin crafts ,gypsum crafts ,unsaturated resin crafts, lighting and candles crafts ,plastic toy , stationery gifts crafts industry, a large statue Buddha, relievo furniture, furniture decorative materials,  and so on.

RTV-2 silicone for molding plaster statues operations:
If the customer wants to make large products and large size molds, the mold should be made of silicon rubber with high hardness. On the contrary, if the mold with fine and precision  patterns, it should be made of silicon with low hardness. The amount of the curing agent depends on the actual requirements of the customer. If molds requiring fast drying and demould, more curing agent is needed; contrarily, if molds requiring slower drying and demould, less curing agent is needed.
(Note: our company does not recommend you to add silicone oil. If a special soft silicon mold or fine detailed and complex patterns products are required, 5%-10% silicone oil can be added to soften the mold for easy demould.)

Frequently asked questions of moulding silicone rubber:
Why does the mold made of silicone rubber  have an unsmooth surface with tracks and strips on it?
It is due to product or model to be molded should hasn't been sanded or polished . If the mold or product is not sanded or polished, the mold made of whatever quality silicone rubber will not be good and smooth enough since the mold or the product itself is not smooth or perfect. Another case is that uneven brushing of the release agent will also bring about unsmoothness of the mold.

Any further information pls feel free to contact with Ms Nina
TEL: 0086-755-89948019
Fax: 0086-755-89948030
E-mail: hyjr(at)szrl(dot)net
Website: www(dot)szrl(dot)net
反对 0举报 0 收藏 0 评论 0
更多>本企业其它产品
网站首页  |  关于我们  |  服务条款  |  广告合作  |  付款方式  |  使用协议  |  联系我们  |  网站地图  |  排名推广  |  广告服务  |  网站留言  |  RSS订阅  |  违规举报